3Flex Surface Area and Porosity Analyzer
BET, 3Flex Micromeritics
Location

147 Stepan Chemistry Hall
Capabilities
- Pressure Measurement Specifications:
- Range: 0 to 950 mmHg
- Resolution: 10-mmHg Transducer - 0.00001 mmHg (Analysis) 1 mmHg (Degas)
- Accuracy: Within 0.15% of reading
- 2 degas ports
- Chemisorption and vapor adsorption options
Typical Use
- Surface area of adsorbents, fine powders, and ceramics
- Macro/Meso/Microporosity
- Chemisorption (metal and oxide catalyst active surface area)
- Pyridine adsorption (acidity/basicity of surface active centers)
Internal Hourly Rates
- Unassisted: $16
- Assisted: $76
External Hourly Rates
- Unassisted: $74
- Assisted: $119
Daily Rates
- Internal Unassisted: $96
- External Unassisted: $444